Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light
|Updated:2026-01-06
|
Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light
Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light
中国化学工程学报(英文版)2012年20卷第5期 页码:895-899
Affiliations:
Institute of Environment of Jiangsu University, Jiangsu University Branch Center of State Key Lab of Urban Water Resource and Environment, Zhengjiang,China,212013
储金宇, 仲蕾. Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light[J]. 中国化学工程学报(英文版), 2012,20(5):895-899.
CHU Jinyu, ZHONG Lei. Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light[J]. Chin.J.Chem.Eng., 2012, 20(5): 895-899.
储金宇, 仲蕾. Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light[J]. 中国化学工程学报(英文版), 2012,20(5):895-899.DOI: 10.1016/S1004-9541(12)60415-7.
CHU Jinyu, ZHONG Lei. Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light[J]. Chin.J.Chem.Eng., 2012, 20(5): 895-899.DOI: 10.1016/S1004-9541(12)60415-7.
Photocatalytic Degradation of Methylene Blue with Side-glowing Optical Fiber Deliverying Visible Light
摘要
Abstract
The side-glowing optical fibers (SOFs) were chosen as the conducting medium of endogenous light; and 20 mg·L
-1
methylene blue was chosen as the target to be degraded. The SOF is made up of quartz core with a silicon cladding
which can emit light through side surface more uniformly and transmit light for longer distance to avoid attenuation of light by liquid medium. The filament lamp was chosen as visible light source. Different reaction conditions
such as the presence of optical fiber or not
the quantity of SOF
light irradiation intensity were tested by measuring the methylene blue degradation of methylene blue. The results show that suitable reaction conditions were 1.167 g·L
-1
Ag
+
/TiO
2
with 7% (by mass) of Ag
+
doped in TiO
2
and 500 roots of SOF (30 cm length in solution). The photocatalytic degradation efficiency under 300W lamp irradiation for 8h was about 97%. And the photocatalytic degradation efficiency of methylene blue degradation was proportional to SOF quantity
light irradiation intensity and catalytic dosage within a certain range. Compared with general UV and visible light SOFs could save a huge amount of energy and cost
in the potential applications in dealing with organic pollutants on a large scale.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.
In-situ construction of morphology-controllable flower-shaped lignin-derived carbon/ZnO composite for efficient photocatalytic degradation of organic dyes
A high H2 evolution rate under visible light of a CdS/TiO2@NiS catalyst due to a directional electron transfer between the phases
Enhanced photocatalytic H2O2production by morphology-controlled CdS nanocatalysts
Immobilization strategies, supporting materials, and performance advantages of photocatalysts in ammonia synthesis
Boosting high-energy-density zinc-ion capacitors with an ultra-stable redox mediator
相关作者
Zhengtao Wei
Xiaofei Wang
Xuliang Lin
Xueqing Qiu
Jianling Meng
Yongdan Li
Zhang Qixin
Yang Yifan
相关机构
Guangdong Basic Research Center of Excellence for Ecological Security and Green Development, Guangdong University of Technology
Guangdong Provincial Laboratory of Chemistry and Fine Chemical Engineering Jieyang Center
Guangdong Provincial Key Laboratory of Plant Resources Biorefinery, School of Chemical Engineering and Light Industry, Guangdong University of Technology
2 Tianjin Key Laboratory of Applied Catalysis Science and Technology, State Key Laboratory for Chemical Engineering, School of Chemical Engineering, Tianjin University
Key Laboratory of Marine Chemistry Theory and Technology of Ministry of Education, Ocean University of China